TECHNICAL DATA
Item
|
Parameters
|
Appearance
|
Light to dark liquid
|
Kinematic viscosity, (40ºC) mm2 /s
|
Actual measured value
|
Density (20ºC) kg/m³
|
800-1200
|
PH
|
≥7
|
PRODUCT DESCRIPTION
Delayed coking corrosion inhibitor is mainly used at fractionating tower of coke unit in oil refinery.
FEATURES
(1) Good water solubility, does not affect the oil quality after use;
(2) Happen physical adsorption, chemical adsorption and complexing film on the metal surface , high corrosion rate
(3) Compounded by a variety of additives, applicable for wide range temperature.
APPLICATION METHOD
The injecting amount is about 60-100ppm, and should be doubled in the initial month.
NOTICE
(1) The product should be stored in ventilated, cool and dry warehouse.
(2) In the application, the user should select the best conditions according to the actual situation of the factory.